Flux baths made with zinc chloride and ammonium chloride put dissolved Zn²⁺ and NH₄⁺ into the rinse water. A pH-driven precipitation step, followed by biological polishing, cuts zinc by about 93–95% and ammonia by up to 98%. The numbers and the caveats are below.
The fluxing stage in galvanizing uses concentrated zinc chloride (ZnCl₂) and ammonium chloride (NH₄Cl). Therefore the rinse water that follows carries high dissolved zinc (Zn²⁺) and ammonium (NH₄⁺). EPA documentation notes kettle‑flux baths can be ≈98% ZnCl₂ by weight (nepis.epa.gov). It also notes that galvanizing rinse waters contain “zinc, lead, and iron, which must be treated as hazardous” (nepis.epa.gov).
That chemistry meets hard policy. Indonesian discharge regulations (PermenLH/PermenLHK) set low mg/L limits for heavy metals. For example, zinc is usually ≲5 mg/L. They also restrict ammonia‑nitrogen to the low mg/L range (drawing on values cited in Ratnawati. We infer similar targets might apply for galvanizing effluent) (researchgate.net).
There is a playbook that works. Start with pH‑driven chemical precipitation of zinc as zinc hydroxide. Then add biological treatment if very low ammonia is needed. Below is what the data say about setpoints, removals, and unit process sizing, and what it means for compliance.
Fluxing rinse composition and standards
Flux rinses are heavy-metal wastewater. They contain a lot of dissolved Zn²⁺ and NH₄⁺ because fluxing uses ZnCl₂ and NH₄Cl (nepis.epa.gov). Even dilute rinses can carry tens of mg/L Zn when the upstream kettle-flux is very concentrated (nepis.epa.gov). EPA also classifies galvanizing rinse water as hazardous because of its zinc, lead and iron content (nepis.epa.gov). The Indonesian Ministerial standards cited in Ratnawati put zinc in the low mg/L range. In an Indonesian ZnO-factory case, influent at 79 mg/L Zn was precipitated to 3.7 mg/L (95% removal). That met the Minister's effluent standard (researchgate.net).
Chemical precipitation via pH adjustment
The core step is pH-driven precipitation of Zn²⁺ as Zn(OH)₂. You raise the pH to ~9–10 with Ca(OH)₂ or NaOH (pH is a measure of acidity/alkalinity). This converts Zn²⁺ to solid Zn(OH)₂: Zn²⁺ + 2 OH⁻ → Zn(OH)₂ (researchgate.net). The best pH window is ~9.0–9.5. One study reported 93–95% Zn removal in that range (researchgate.net).
In Ratnawati's tests, adding alkali and 50 mg/L polymer (PAC, polyaluminum chloride coagulant) removed Zn from 79 to 3.71 mg/L (95.3% removal) within 10 minutes at pH 9.5 (researchgate.net). pH 9.0 alone also gave 93.8% removal (Zn ≈4–5 mg/L) and used less reagent (researchgate.net). EPA cites plants that "treated wastewater by lime and polymer addition and pH adjustment" with good results (nepis.epa.gov).
After precipitation, the heavy-metal hydroxides must be settled or filtered. Zn(OH)₂ particles settle slowly, so a coagulant or flocculant is usually added. The settled sludge contains the metal hydroxides (researchgate.net). To control pH accurately in this step, plants often use an automated dosing pump. For coagulation, industrial PAC formulations such as PAC for wastewater are commonly added to grow settleable flocs. [Settling is typically performed in a clarifier](https://beta.co.id/en/blog/inside-a-galvanizing-plants-quench-tank-fix-filters-highph-chemistry-and-a-clarifier-that). Equipment like a clarifier removes suspended solids by detention and gravity separation.
Sludge characteristics and handling
Galvanizing sludge usually contains ~8–18% Zn by dry weight. That concentration is high enough for possible zinc recovery (mdpi.com). For stoichiometry, ~1.5 kg Zn(OH)₂ forms per kg Zn removed. The clarified effluent after solids removal contains mainly calcium and chloride ions. Plants usually dewater and minimize the resulting sludge volume using solutions in the vein of sludge treatment and an industrial filter press.
Ammonia removal and biological polishing
Because the pH step targets metals, ammonia needs a separate lens. Raising pH shifts ammonium (NH₄⁺) to volatile ammonia gas (NH₃) (pKa≈9.25, where pKa is an acid–base equilibrium constant). Therefore some stripping does occur. However, significant ammonia usually remains. If discharge limits are very strict, on the order of a few mg/L NH₃–N, biological nitrification (biological oxidation of NH₄⁺→NO₂⁻→NO₃⁻) is advisable. For planning it, see nutrient removal for industrial wastewater. Full‑scale systems routinely achieve >90% ammonia removal. Even experimental counter‑current aeration configurations have reported 98% removal to <1 mg/L NH₃–N (nepis.epa.gov). Realistic designs, such as SBR (sequencing batch reactor), RBC and MBBR (moving‑bed biofilm reactor), can reduce high ammonia (tens of mg/L) to single‑digit mg/L.
Heavy metals can inhibit nitrifiers. Therefore it is important to remove Zn first (mdpi.com) (mdpi.com). Once Zn is precipitated to ≲5 mg/L, toxicity to nitrifiers is minimal. Zn levels up to ~5 mg/L had little effect on AOB (ammonia‑oxidizing bacteria), but ~20 mg/L caused irreversible inhibition (mdpi.com). Where biological polishing is selected, utilities usually use platforms like SBR or MBBR to get nitrification at a compact footprint.
If permits dictate near‑zero ammonia (for example <1–2 mg/L NH₃–N), integrate nitrification and, if needed, heterotrophic denitrification (biological reduction of NO₃⁻). This rinse water has little BOD and may need external carbon (for example methanol). If financial or land constraints exist, one could consider gas‑stripping towers, which in tests reached similar ammonia removal (nepis.epa.gov). However, a biological reactor is usually more compact and cost‑effective for continuous flows in the context described.
Measured removals and operating ranges
Chemical precipitation can routinely remove >90% of dissolved Zn. In practice, initial Zn around ~80 mg/L dropped to ~3–5 mg/L (≈95%) in controlled studies (researchgate.net) (researchgate.net). Dosage, for instance on the order of 1.1 kg Ca(OH)₂ per kg Zn, and polymer addition in the tens of mg/L should be scaled to the flow and concentration.
For ammonia, aerobic nitrification in reactors of the right size removes more than 90%. The cited counter-current aeration test reached 98% removal, to less than 1 mg/L NH₃–N (nepis.epa.gov).
Sizing example and compliance check
Take 100 m³/day of flux effluent with 80 mg/L Zn and 50 mg/L NH₄–N. Dosing about 10–12 kg/day Ca(OH)₂ (or NaOH) to reach pH 9–9.5 would precipitate about 95% of the Zn, leaving 4 mg/L or less. The Zn(OH)₂ sludge forms at about 1.5 kg per kg Zn removed and must be dewatered. After solids removal, the water with about 50 mg/L NH₄–N enters a biological reactor.
A 500 m³ biological unit with 6–8 h HRT (hydraulic retention time) and DO of about 2 mg/L (dissolved oxygen) could nitrify more than 90%, to less than 5 mg/L NH₄–N, and give about 7 mg/L NO₃–N. In the context described, this performance meets strict limits in most jurisdictions. These data, 95% Zn removal (researchgate.net) and about 98% NH₃ removal (nepis.epa.gov), guide realistic sizing and compliance evaluation.
Sources and validation
We took the findings on flux composition and hazardous characterization from EPA reports (nepis.epa.gov and nepis.epa.gov). Ratnawati et al. (2020) show Zn precipitation at pH 9–9.5 with ≥95% removal. They also show that 50 mg/L polymer (PAC) speeds up turbidity removal (researchgate.net and researchgate.net). EPA guidance also notes lime–polymer treatment of galvanizing effluent (nepis.epa.gov). The nitrification and stripping benchmarks come from U.S. EPA data (nepis.epa.gov). We summarized the metal toxicity thresholds for nitrifiers and the sludge zinc content from MDPI sources (mdpi.com, mdpi.com and mdpi.com). The regulatory context comes from Indonesian MOE regulations cited in Ratnawati (researchgate.net) and from general practice, for example a Zn effluent of about 5 mg/L. Each design choice (pH setpoint, coagulant dose, reactor size) needs validation by lab tests or pilot trials on the actual flux wastewater.