WhatsApp

Poly aluminium chloride (PAC)

PAC Supplier in Indonesia for WTP & WWTP

Updated

PAC supplier in Indonesia for liquid and powder BETAGARD grades. Compare Al₂O₃, insolubles, packaging, jar tests, delivery, and treatment cost per m³.

PAC Supplier in Indonesia for WTP & WWTP

Discuss the application.

Send the application, operating conditions and the result you expect. Our team will discuss the options with you.

Ask about this product

or use the contact page

PT Beta Pramesti Asia is a PAC supplier in Indonesia for liquid and powder BETAGARD grades used in industrial water and wastewater treatment. Buyers should shortlist the grade by published Al₂O₃ content, insoluble limit, packaging, storage and dosing setup. Then confirm the dose with the actual water.

Last technically reviewed: 1 August 2026.

Which BETAGARD Poly Aluminium Chloride Grade Should a Buyer Test?

Start with the product form you need, the Al2O3 specification, the insoluble limit, and the storage and dosing arrangement. Then compare performance in a jar test. The table is a procurement shortlist. It does not replace testing with the actual feed water, the downstream process and the sludge-handling conditions.

GradeFormPublished Al2O3 specificationPublished insoluble specificationAvailable packaging
BETAGARD 4008Clear to yellowish liquidMin. 8%Not stated on this page25 or 30 kg bucket; 220 kg drum; 1,200 kg tote
BETAGARD 4010Clear to yellowish liquidMin. 10%Not stated on this page25 or 35 kg bucket; 240 kg drum; 1,200 kg tote or tank
BETAGARD 4012Clear to yellowish liquidMin. 12%Not stated on this page25 or 35 kg bucket; 240 kg drum; 1,200 kg tote or tank
BETAGARD 4031White powderMin. 28%Max. 0.5%25 kg bag
BETAGARD 4033Yellow powderMin. 28%Max. 1.5%25 kg bag

What Should a Polyaluminium Chloride Supplier Put in the Quotation?

A useful quotation identifies the exact BETAGARD grade, specification and packaging. It then separates product supply from testing, delivery, unloading and application support. This lets a buyer compare like-for-like offers. It also lets the buyer calculate treatment cost from a jar-tested commercial-product dose, not from product price alone.

Quotation evidenceDetails to requestBuyer decision supported
Product identity and qualityBETAGARD grade, form, published Al₂O₃ and insoluble limits, TDS, SDS and batch CoAConfirms that the material delivered matches the material evaluated
Commercial basisNet quantity, package size, price basis, validity, taxes and delivery destinationCreates a comparable delivered-cost basis
Test basisWater sample, dose range, mixing sequence, outlet targets and sludge observationsConverts the shortlisted grade into a defensible cost per m³
Supply planMonthly demand, lead time, unloading access, storage capacity and safety stockTests whether the proposed delivery pattern fits plant operation
Work boundarySampling, jar testing, pump calibration, plant trial, reporting and follow-upPrevents technical support from being assumed but left unpriced

For a broader powder-versus-liquid procurement comparison, use the PAC coagulant buyer page. Send the water data, monthly requirement and delivery location through the Beta Pramesti Asia contact page.

How should liquid and powder PAC be compared for cost per m³?

Compare liquid PAC and powder PAC at the same treated-water result, not by price per kilogram alone. Before deciding the treatment cost per m³, buyers should calculate the commercial-product dose, Al₂O₃ content, make-down needs, freight, handling loss, tank requirements and sludge impact.

Comparison basisLiquid PACPowder PAC
Dosing readinessEasier to feed directly from a tank or toteRequires make-down, agitation, and dust control
Logistics costShips water in the product, but handling is simplerMore concentrated, but needs reliable dissolution facilities
Operating riskCheck tank material, containment, and transfer linesCheck solubility, ageing time, dust, and solution concentration
Acceptance evidenceJar test and plant trial at the as-supplied doseJar test, make-down repeatability, and plant trial with the actual solution

BETAGARD PAC Grade Details

BETAGARD 4008

BETAGARD 4008 is a Poly Aluminium Chloride (PAC) coagulant and sludge conditioner for liquid-solid separation. In water and wastewater treatment, it is evaluated for separating suspended solids, colour, natural organic matter and colloidal clay from the water phase.

Technical Specifications

Product% Al2O3AppearanceSpecific gravitypH 1%Dosage & Usage InstructionsHandling PrecautionsPackaging
BETAGARD 4008Min 8%Clear to yellowish liquid1.10 - 1.203.0 - 5.0Determine dosage by laboratory jar test and confirm it in a plant trial.BETAGARD 4008 is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics and other more resistant materials. Galvanized equipment should not be used. Tightly close drum containers after use. See MSDS for additional information.Available in 25, 30 KG per bucket, 220 KG per plastic drum or 1200 KG per tote.

BETAGARD 4010

BETAGARD 4010 is a Poly Aluminium Chloride (PAC) coagulant and sludge conditioner for liquid-solid separation. It is evaluated for separating suspended solids, colour, natural organic matter and colloidal clay in water and wastewater treatment.

Technical Specifications

Product% Al2O3AppearanceSpecific gravitypH 1%Dosage & Usage InstructionsHandling PrecautionsPackaging
BETAGARD 4010Min 10%Clear to yellowish liquidMin 1.193.5 - 5.0Determine dosage by laboratory jar test and confirm it in a plant trial.BETAGARD 4010 is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics and other more resistant materials. Galvanized equipment should not be used. Tightly close drum containers after use. Refer to MSDS for additional information.Available in 25, 35 KG per bucket, 240 KG per plastic drum or 1200 KG per tote or tank.

BETAGARD 4012

BETAGARD 4012 is a Poly Aluminium Chloride (PAC) coagulant and sludge conditioner for liquid-solid separation. It is evaluated for separating suspended solids, colour, natural organic matter and colloidal clay in water and wastewater treatment.

Technical Specifications

Product% Al2O3AppearanceSpecific gravitypH 1%Dosage & Usage InstructionsHandling PrecautionsPackaging
BETAGARD 4012Min 12%Clear to yellowish liquid1.19 - 1.403.5 - 5.0Determine dosage by laboratory jar test and confirm it in a plant trial.BETAGARD 4012 is mildly acidic, stable under ordinary conditions. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics and other more resistant materials. Galvanized equipment should not be used. Tightly close drum containers after use. Refer to MSDS for additional information.Available in 25, 35 KG per bucket, 240 KG per plastic drum or 1200 KG per tote or tank.

BETAGARD 4031

BETAGARD 4031 is the white powder grade in this series. It has a published minimum Al₂O₃ content of 28% and a maximum insoluble content of 0.5%. Evaluate it with the actual water, the preparation method, the separation unit and the finished-water target.

Technical Specifications

ProductAppearance% Al2O3pH 1%InsolubleDosage & Usage InstructionsHandling PrecautionsPackaging
BETAGARD 4031White powderMin 28%3.5 - 5.0Max. 0.5%The actual dosage of BETAGARD 4031 should be determined by laboratory tests or factory trials. Consult the technical team.BETAGARD 4031 is moderately acidic, stable under ordinary conditions. Avoid use in galvanizing equipment. Close container after use and store in a suitable place.Available in packs of 25 kg per bag.

BETAGARD 4033

BETAGARD 4033 is the yellow powder grade in this series. Its published minimum Al₂O₃ content is 28% and its maximum insoluble content is 1.5%. Evaluate it on the same water and acceptance criteria as the other candidates. Then form, dose, sludge and treatment cost stay comparable.

Technical Specifications

ProductAppearance% Al2O3pH 1%InsolubleDosage & Usage InstructionsHandling PrecautionsPackaging
BETAGARD 4033Yellow powderMin 28%3.5 - 5.0Max. 1.5%The actual dosage of BETAGARD 4033 should be determined by laboratory tests or factory trials. Consult the technical team.BETAGARD 4033 is moderately acidic, safe to use under ordinary conditions. Avoid use on galvanizing equipment. Store product in a cool, dry place.Available in 25 kg bags.

Typical Applications

  • Raw-water clarification: Screen liquid and powder grades by jar testing before sedimentation or filtration. Record turbidity, colour, pH, alkalinity, floc formation, settled-water quality, and sludge.
  • Industrial wastewater treatment: Evaluate PAC for suspended solids, turbidity, colour, or selected precipitable contaminants. Performance depends on contaminant form, pH, treatment aids, and the separation unit.
  • Pulp and paper water circuits: Test the actual white-water or effluent stream. Include fibre/filler recovery, downstream reuse quality, and sludge handling in the acceptance criteria.
  • Phosphorus treatment: Use a treatability test to establish chemical demand, pH response, residual aluminium where relevant, sludge production, and compliance with the facility’s actual discharge limit.
  • Dissolved Air Flotation (DAF): Test the dose and floc condition upstream of DAF. Then verify TSS or FOG separation, floated-sludge handling, and chemical cost at operating flow.
  • Sludge conditioning: Compare dewaterability, polymer demand, filtrate or centrate quality, and dry-solids handling before changing the programme.

Compatible Products

  • Dissolved Air Flotation (DAF): Evaluate coagulation and flotation together when the target includes fine solids, oil, or grease.
  • Betaqua Ultrafiltration: Coagulant-enhanced pretreatment may be screened before UF only after the membrane limits, residuals, backwash, and cleaning method are defined.
  • Moving Bed Bioreactors (MBBR): A physical-chemical stage may precede MBBR where the design needs upstream solids or colloid removal.

Installation Context

The liquid and powder package sizes published for each grade are listed above. Confirm storage and transfer materials against the current TDS and SDS. For powder, document the make-down concentration, dilution-water quality, agitation, ageing or hold time where specified, and dust controls. For liquid, define unloading, containment, tank working volume, transfer line, pump range and calibration method.

There is no universal PAC dose or storage-tank size. Find the dose by jar testing representative water. Then confirm it in a controlled plant trial. The trial records product batch, actual feed rate, flow, outlet quality, sludge response and cost per m³. Send that basis through the Beta contact page for a grade and supply review.