Oilfield chemicals
Pour Point Depressant for Crude Oil
Updated
BETAFLOW pour point depressant lowers crude-oil pour point and controls paraffin in pipelines. Compare PP 103 and 9500 using oil tests and field data.
Discuss the application.
Send the application, operating conditions and the result you expect. Our team will discuss the options with you.
PT Beta Pramesti Asia supplies the BETAFLOW PP Series for crude-oil flow assurance programs. The formulations act as pour point depressants. They lower the crude-oil pour point and also help inhibit wax formation and disperse paraffin deposits. Therefore the oil stays pumpable through pipelines.
Product selection, including BETAFLOW PP 103 or BETAFLOW 9500 Series, must be matched to the crude-oil characteristics, wax appearance temperature, temperature profile and field operating conditions.
Last technically reviewed: 30 July 2026.
What Is a Pour Point Depressant?
A pour point depressant (PPD) is a chemical that lowers the minimum temperature at which oil can still flow. It changes how wax crystals grow and how they are structured. Therefore the crystals are less likely to form a rigid network that increases viscosity or restricts the flow line.
Pour point depressant and paraffin dispersant are two different functions. A PPD focuses on lowering pour point and changing the wax crystals. A paraffin dispersant helps keep paraffin particles suspended in the oil and reduces their adhesion to pipeline surfaces. One formulation can provide both functions.
Which BETAFLOW Pour Point Depressant Should Be Trialled?
Trial BETAFLOW PP 103 when the main objective is pour-point reduction and wax-crystal control. Trial BETAFLOW 9500 when the program also needs paraffin dispersion. However, do not choose either from the page alone. Representative crude-oil testing, the pipeline temperature profile, injection location, chemical compatibility and field acceptance criteria must govern the trial.
| Buyer question | BETAFLOW PP 103 | BETAFLOW 9500 Series |
|---|---|---|
| Published function on this page | Pour-point reduction and paraffin-crystallisation control | Pour-point reduction plus paraffin dispersion |
| Application described | Continuous injection | Continuous or batch injection |
| Dose information | Initial 500–5,000 ppm range; optimise by laboratory test and field trial | Select from crude-oil testing and wax-crystallisation temperature |
| Procurement detail | 200-litre drum | Review the BETAFLOW 9500 technical data sheet |
| Evidence needed before selection | Pour point, viscosity response, temperature profile, compatibility, and field acceptance criteria | Deposit type, pour point, temperature profile, dispersion response, compatibility, and field acceptance criteria |
BETAFLOW PP 103
BETAFLOW PP 103 helps prevent paraffin crystallization by lowering the pour point. Therefore different crude oils stay mobile at lower operating temperatures.
Product Benefits
- Lowers crude-oil pour point.
- Helps maintain flow at lower temperatures.
- Reduces the tendency to form rigid wax deposits.
- Helps reduce transfer-pump load.
- Supports stable crude-oil production rates.
- Compatible with other production chemicals after compatibility testing.
BETAFLOW PP 103 Specifications
| Parameter | Details |
|---|---|
| Physical form and odor | Yellow-to-brown liquid with an aromatic-solvent odor |
| Density | 0.865 ± 0.1 g/cc |
| Application method | Continuous injection into the system |
| Initial dosage range | 500–5,000 ppm based on produced-oil volume; the actual dosage must be optimized through laboratory testing and a field trial |
| Packaging | 200-liter drum |
BETAFLOW 9500 Series
BETAFLOW 9500 Series is a crude-oil pour point depressant. It also helps disperse paraffin deposits into the produced oil when applied continuously. The formulation supports lower pour point, inhibition of paraffin formation and reduced wax deposition in production systems.
It can be applied through continuous or batch injection. Application conditions and dosage must be selected from crude-oil testing and the wax crystallization temperature.
Download the BETAFLOW 9500 Series technical data sheet.
Crude-Oil Pipeline Applications
A BETAFLOW PP program can be considered for:
- Wellheads and crude-oil flow lines.
- Transfer pipelines and production gathering systems.
- Paraffinic crude oil with a high risk of wax formation.
- Low-temperature operations or pipelines where the temperature drops a lot.
- Systems that need both pour point control and paraffin dispersion.
In one field application, BETAFLOW 9500 was injected continuously at the wellhead. This helped restore crude-oil flow to 100% capacity and reduced how frequently the pipeline needed maintenance. Read the BETAFLOW 9500 paraffin-control case study.
Frequently Asked Questions
Is “pour point dispersant” the correct term?
The standard technical term is pour point depressant because its main job is to lower pour point. When a product also disperses wax or paraffin, that job is better described as a paraffin dispersant.
Is a pour point depressant the same as a wax dissolver?
No. A pour point depressant changes how the wax crystallizes and keeps the crude oil moving. A wax dissolver is used to dissolve deposits that have already formed. Program selection depends on the deposit conditions and what the treatment needs to achieve.
How is the BETAFLOW PP dosage selected?
Dosage should not be chosen from a general range alone. You need crude-oil analysis, pour point testing, the temperature profile, the injection location and a field trial to choose the right product and dosage.
Discuss Your Flow Assurance Program
Contact the PT Beta Pramesti Asia technical team to evaluate your crude oil, the paraffin-deposition risk and the injection location, and to find the most suitable BETAFLOW PP program.