Information
Oilfield Chemicals BETAFLOW Series for Oil and Gas Industry
Complete reference for BETAFLOW Series oilfield chemicals for corrosion, scale, demulsifier, biocide, oxygen scavenger, H2S scavenger, antifoam, dewaxing, and pipeline needs.
Updated
Oilfield Chemicals: Referensi Lengkap Produk Kimia untuk Operasi Migas
Oilfield chemicals are a group of special chemicals used to support exploration, production, processing, transport and maintenance of oil and gas facilities. In the oil and gas industry, problems such as corrosion, scaling, foam, emulsions, wax/paraffin, bacteria, sour gas and falling flow efficiency in pipelines can cause downtime, equipment damage, lower production and higher operating costs.
Therefore, choosing the right oilfield chemicals is an important part of keeping the production system reliable. PT Beta Pramesti Asia supplies the BETAFLOW Series, made for oilfield, refinery, gas treatment, pipeline, water injection, produced water treatment and other oil and gas support facilities.
Apa Itu Oilfield Chemicals?
Oilfield chemicals are technical chemicals formulated to help control operating problems in oil and gas fields. They are used in crude oil production systems, gas plants, water injection, refineries, pipelines, separators, storage tanks, produced water treatment facilities and gas dehydration units.
The main functions of oilfield chemicals include:
- Inhibiting corrosion in pipes, separators, tanks and process equipment.
- Preventing scale such as calcite, gypsum and other mineral deposits.
- Reducing dissolved oxygen in water injection and hydrotest systems.
- Controlling foam in separators and oil/gas production systems.
- Breaking oil-water emulsions so separation works better.
- Removing or controlling wax, paraffin and heavy hydrocarbon deposits.
- Helping treat produced water and refinery wastewater.
- Controlling bacteria, including sulphate reducing bacteria.
- Improving pipeline flow efficiency with drag reducing agents.
- Supporting gas treatment, gas dehydration and CO2 removal.
Peran Oilfield Chemicals dalam Industri Minyak dan Gas
In the oil and gas industry, chemical treatment is not just an additive. It is part of the operating strategy that keeps the system performing. Without the right chemical treatment, equipment can fail sooner, pipelines can plug, and oil-water separation can run poorly.
Oilfield chemicals help operators keep the process stable from the production well, surface facilities, water injection system and pipeline through to the refinery and gas processing units. The right chemicals help cut maintenance costs, make equipment last longer and keep production quality.
Jenis Oilfield Chemicals BETAFLOW Series
PT Beta Pramesti Asia supplies a range of BETAFLOW Series products for oilfield and oil and gas facility needs. Below is a product reference by function and application.
1. BETAFLOW 8080 Series - Antifoam
Foam in separators, gas treatment and production systems can cause carryover. It lowers separation efficiency and disturbs stable operation. Foam that is not controlled can make level readings inaccurate, reduce separator capacity and raise the risk of contamination between phases.
BETAFLOW 8080 Series - Antifoam is a silicone oil based antifoam that can be used in oil and aqueous systems. It works as a defoamer to break foam quickly, or as an antifoam to prevent foam over time.
Aplikasi BETAFLOW 8080 Series antara lain:
- Oil and gas separator.
- Drilling operation.
- Cementing operation.
- Aqueous and oil-based fluid systems.
- Processes with high temperature and pressure conditions.
This product helps keep the separation process stable, reduces operational problems caused by foam and supports the efficiency of oil and gas production systems.
Download PDF BETAFLOW 8080 Series - Antifoam
2. BETAFLOW 9120 Series - Corrosion Inhibitor Oil Soluble
Corrosion is one of the main problems in oil and gas operations. Corrosion can come from HCl, carbonic acid, H2S, CO2, dissolved oxygen, biological deposit and aggressive fluid conditions.
BETAFLOW 9120 Series - Corrosion Inhibitor OS is an oil soluble corrosion inhibitor. It helps protect metal surfaces from corrosion in production, drilling, crude oil transportation and refining systems.
This product works by forming a protective layer on the metal surface, so direct contact between the corrosive fluid and the metal is reduced. With the right protection, the risk of pipe leaks, equipment damage and downtime can be reduced.
Aplikasi BETAFLOW 9120 Series antara lain:
- Oil production system.
- Crude oil transportation.
- Drilling operation.
- Refining crude oil.
- Systems that need an oil soluble corrosion inhibitor.
Download PDF BETAFLOW 9120 Series - Corrosion Inhibitor OS
3. BETAFLOW 9121 Series - Corrosion Inhibitor
BETAFLOW 9121 Series - Corrosion Inhibitor is formulated to help control corrosion in refinery, petrochemical processing and oilfield equipment. This product forms a protective film on the metal surface, so it can reduce the corrosion rate and make the equipment last longer.
A corrosion inhibitor such as BETAFLOW 9121 Series is important in systems that handle corrosive fluids, especially when CO2, H2S, oxygen or high water content is present. With the right chemical treatment, a company can reduce maintenance costs and the risk of unplanned shutdown.
Aplikasi BETAFLOW 9121 Series antara lain:
- Refinery process.
- Petrochemical processing.
- Oilfield equipment.
- Pipeline and piping system.
- Separator and vessel.
- Oil and gas production systems that need corrosion protection.
Download PDF BETAFLOW 9121 Series - Corrosion Inhibitor
4. BETAFLOW 9121 Series - Corrosion Inhibitor Water Soluble
Corrosion inhibitor needs can differ from the oil soluble type, depending on the fluid and the system. BETAFLOW 9121 Series - Corrosion Inhibitor Water Soluble is suitable for applications that need a water soluble inhibitor.
This product helps protect systems that carry a lot of water, such as water injection, produced water, hydrotest water and other aqueous systems. The chemical forms a protective layer on metal surfaces and reduces the risk of corrosion from oxygen, CO2, H2S and other corrosive contaminants.
Aplikasi BETAFLOW 9121 Water Soluble antara lain:
- Water injection system.
- Produced water system.
- Hydrotest water.
- Piping and equipment that carry aqueous fluid.
- Oil and gas systems that need a water soluble corrosion inhibitor.
Download PDF BETAFLOW 9121 Series - Corrosion Inhibitor Water Soluble
5. BETAFLOW 9122 Series - Corrosion Inhibitor PF
BETAFLOW 9122 Series - Corrosion Inhibitor PF is a filming inhibitor used to protect steam and gas lines in oil and petrochemical plants. The product works by forming a protective film on the metal surface, so corrosive fluids do not attack the equipment surface directly.
This product is relevant for areas at risk of corrosion in steam lines, gas lines and process systems with demanding operating conditions.
Manfaat BETAFLOW 9122 Series antara lain:
- Helps protect steam lines and gas lines.
- Reduces the risk of corrosion in oil and petrochemical plants.
- Helps keep process systems reliable.
- Reduces the risk of downtime from equipment damage.
Download PDF BETAFLOW 9122 Series - Corrosion Inhibitor PF
6. BETAFLOW 9123 Series - Corrosion Inhibitor Multitreat OSWD
BETAFLOW 9123 Series - Corrosion Inhibitor Multitreat OSWD is a corrosion inhibitor that is oil soluble and water dispersible. The product is designed for oil production and water injection systems.
Because it is oil soluble and water dispersible, the product can be used in systems that involve both oil and water phases. It helps protect pipelines, production systems and equipment that carry oil and gas fluids against corrosion.
Aplikasi BETAFLOW 9123 Series antara lain:
- Oil production system.
- Water injection system.
- Pipeline.
- Surface facility.
- Systems with a combination of oil and water phase.
Download PDF BETAFLOW 9123 Series - Corrosion Inhibitor OSWD
7. BETAFLOW 9130 Series - Scale Inhibitor
Scale is a mineral deposit that forms when the chemistry of produced water or injection water is unstable. Scale such as gypsum, calcite and other complex deposits can reduce flow capacity, plug pipes, disturb wellhead equipment and lower production efficiency.
BETAFLOW 9130 Series - Scale Inhibitor is formulated with organic deposit control compound, complex polymers and organic sequestrants. The product works by stopping micro crystal scale from growing before it forms a larger crystal lattice.
Manfaat scale inhibitor antara lain:
- Stops scale from forming in production systems.
- Helps keep equipment surfaces clean.
- Reduces the risk of plugging in pipes and equipment.
- Supports production and water injection efficiency.
- Reduces the need for cleaning and maintenance from mineral deposits.
Aplikasi BETAFLOW 9130 Series antara lain:
- Oilfield water system.
- Water injection.
- Produced water.
- Pipeline.
- Wellhead equipment.
- Surface facility.
Download PDF BETAFLOW 9130 Series - Scale Inhibitor
8. BETAFLOW 9131 Series - Chelating Agent
BETAFLOW 9131 Series - Chelating Agent is used in stimulation treatment, cleaning surface facilities, scale removal, and drilling fluid maintenance. In acid treatment or scale-removal treatment, some compounds can dissolve in the treatment fluid. When the pH rises, the reaction products can settle and form an insoluble mass. This can cause permanent damage to the permeability of the formation.
The chelating agent keeps the ions in soluble form so they come out during the cleanup process. This product is important for well workover, intervention process, surface facility cleaning, and preventing the deposition of compounds that can damage the formation.
Aplikasi BETAFLOW 9131 Series antara lain:
- Stimulation treatment.
- Scale removal.
- Cleaning surface facility.
- Drilling fluid treatment.
- Well workover and intervention.
- Prevention of reaction product precipitation.
Download PDF BETAFLOW 9131 Series - Chelating Agent
9. BETAFLOW 9140 Series - Oxygen Scavenger
Dissolved oxygen in water can speed up corrosion, especially in water injection systems and hydrostatic tests. If it is not controlled, dissolved oxygen can damage pipes, tanks, vessels, and process equipment.
BETAFLOW 9140 Series - Oxygen Scavenger is based on sodium bisulphite and is designed to remove dissolved oxygen and certain oxidising elements from fresh water and formation water.
This product is usually applied by continuous dosing with a dosing pump. The oxygen scavenger helps lower the corrosion risk in pipes, tanks, and equipment that contact the injection water directly.
Aplikasi BETAFLOW 9140 Series antara lain:
- Water injection system.
- Hydrostatic test.
- Fresh water system.
- Formation water.
- Pipeline and tank protection.
- Aqueous systems that are sensitive to dissolved oxygen.
Download PDF BETAFLOW 9140 Series - Oxygen Scavenger
10. BETAFLOW 9150 Series - H2S Scavenger
Hydrogen sulfide or H2S is a toxic and corrosive gas that can create safety risks and speed up equipment damage. The H2S in sour gas, sour crude, and produced fluid must be controlled with the right treatment.
BETAFLOW 9150 Series - H2S Scavenger is used to help bind or lower the H2S content in oil and gas production systems. The H2S scavenger is important to lower the risk of odour, toxicity, and corrosion caused by H2S.
Aplikasi BETAFLOW 9150 Series antara lain:
- Sour gas treatment.
- Sour crude treatment.
- Produced fluid system.
- Oil and gas production facility.
- Systems with a risk of H2S exposure.
- Pipeline and surface equipment.
Download PDF BETAFLOW 9150 Series - H2S Scavenger
11. BETAFLOW 9300 Series - Demulsifier
In oil production, oil and water emulsions can form because of natural surfactants, asphaltene, resin, solid particles, or process turbulence. A stable emulsion makes the oil-water separation process harder and can affect the quality of the crude oil and the produced water.
BETAFLOW 9300 Series - Demulsifier is designed to help break the emulsion, speed up free water knockout, and improve the efficiency of the separation process at oil production facilities.
Aplikasi BETAFLOW 9300 Series antara lain:
- Separator.
- Gun barrel tank.
- High pressure treater.
- Electric treater.
- Non-electric treater.
- Crude oil dehydration.
- Oil-water separation process.
Manfaat penggunaan demulsifier antara lain:
- Speeds up the separation of oil and water.
- Improves crude oil quality.
- Reduces water carryover in the crude.
- Helps lower the load on downstream processes.
- Improves the efficiency of separators and treaters.
Download PDF BETAFLOW 9300 Series - Demulsifier
12. BETAFLOW 9310 Series - Deoiler / Reverse Demulsifier
For the produced water side, dispersed oil needs to be separated so the water quality meets the needs of the next process or the discharge standard. Oil in the form of small droplets is usually hard to separate without chemical treatment.
BETAFLOW 9310 Series - Deoiler / Reverse Demulsifier helps oil droplets in effluent water agglomerate, both in oilfield and in refinery discharge.
The product works by helping overcome the static forces that hold small oil droplets in the water. Therefore the droplets can join into larger globules and are easier to separate by flotation or skimming.
Aplikasi BETAFLOW 9310 Series antara lain:
- Produced water treatment.
- Refinery wastewater.
- IAF unit.
- DAF unit.
- API separator.
- Parallel plate interceptor.
- Oil skimming vessel.
Download PDF BETAFLOW 9310 Series - Deoiler Reverse Demulsifier
13. BETAFLOW 9400 Series - Oil Spill Dispersant
An oil spill is a condition that needs fast handling so the impact on the environment and on operations can be reduced. Oil that forms a slick on the water surface is harder to break down if it is not dispersed.
BETAFLOW 9400 Series - Oil Spill Dispersant is a nonionic and anionic liquid compound. It is used to help emulsify and disperse oil spills in water and on solid surfaces.
The product helps form an oil-in-water emulsion. Therefore the oil disperses more easily and natural biodegradation runs faster than on an oil slick that is not treated.
Aplikasi BETAFLOW 9400 Series antara lain:
- Oil spill at sea.
- Oil spill in port areas.
- Ship decks.
- Docks and piers.
- Structures contaminated with oil.
- Industrial areas that need oil spill control.
Download PDF BETAFLOW 9400 Series - Oil Spill Dispersant
14. BETAFLOW 9500 Series - Pour Point Depressant
In crude oil with a high wax/paraffin content, low temperature can make paraffin crystals form and join together. This raises the pour point, lowers flowability and can block pipes and production facilities.
BETAFLOW 9500 Series - Pour Point Depressant is formulated to inhibit paraffin deposit formation, change the wax crystal structure and help keep the crude oil flowing more easily.
Manfaat BETAFLOW 9500 Series antara lain:
- Helps lower the pour point of crude oil.
- Inhibits paraffin deposit formation.
- Helps keep the crude oil flowing.
- Reduces the risk of pipeline blockage.
- Supports flow assurance in production and transport systems.
Download PDF BETAFLOW 9500 Series - Pour Point Depressant
15. BETAFLOW 9501 - Pour Point Depressant
BETAFLOW 9501 - Pour Point Depressant is a pour point depressant that helps solve problems with paraffinic crude, condensate and wax deposit. The product works by modifying the wax crystal structure so the crystals do not join easily and do not form a solid deposit.
Aplikasi BETAFLOW 9501 antara lain:
- Crude oil pipeline.
- Producing well.
- Storage tank.
- Flowline.
- Crude oil systems with high wax/paraffin content.
- Condensate and heavy hydrocarbon streams.
The right pour point depressant helps keep crude oil pumpable, especially at low temperatures or in systems with a high risk of wax deposition.
Download PDF BETAFLOW 9501 - Pour Point Depressant
16. BETAFLOW 9600 Series - Biocide
Bacteria in oilfield systems can cause biofilm, microbiological corrosion, souring, plugging and a drop in system efficiency. One of the bacteria usually targeted by treatment is sulphate reducing bacteria.
BETAFLOW 9600 Series - Biocide is a broad-spectrum bactericide. It works fast and is effective against biofilm because it penetrates well. This product is recommended to control aerobic and anaerobic bacteria in oilfield systems.
Aplikasi BETAFLOW 9600 Series antara lain:
- Water injection system.
- Produced water system.
- Oilfield water system.
- Pipeline and tank.
- Systems at risk of microbial corrosion.
- Systems at risk of souring from bacteria.
Manfaat penggunaan biocide antara lain:
- Controls bacterial growth.
- Reduces the risk of biofilm.
- Reduces the risk of microbiologically influenced corrosion.
- Helps keep injection water quality.
- Reduces the risk of plugging from microbiological activity.
Download PDF BETAFLOW 9600 Series - Biocide
17. BETAFLOW 9700 Series - TEG Formulated
A gas dehydration unit that uses a glycol system needs maintenance to keep working well. Scale deposits, tarry hydrocarbon and other contaminants can disturb the performance of the unit and lower the efficiency of the dehydration process.
BETAFLOW 9700 Series - TEG Formulated is used together with Dehy Acid Cleaner to clean a glycol gas dehydration unit. This product helps remove scale and tarry hydrocarbon without causing channeling of the gas flow through the tray.
Aplikasi BETAFLOW 9700 Series antara lain:
- Glycol gas dehydration unit.
- Gas treatment facility.
- Cleaning system for TEG unit.
- Maintenance of gas processing facilities.
This product helps keep the gas dehydration unit working well, so the removal of water from the gas stays stable and efficient.
Download PDF BETAFLOW 9700 Series - TEG
18. BETAFLOW 9800 Series - Dewaxing Agent
Wax and paraffin deposits can cause serious problems in oil production systems. These deposits can block pipes, lower the flow rate, disturb pumps and increase the frequency of cleaning and maintenance.
BETAFLOW 9800 Series - Dewaxing Agent, or paraffin solvent, works as a wax crystal modifier for crude oil and heavy fuel oil. This product helps prevent agglomeration of paraffin crystals, disperses the paraffin into the oil, and helps keep crude oil pumpable without forming wax deposits that disturb the system.
Aplikasi BETAFLOW 9800 Series antara lain:
- Producing wells.
- Oil handling equipment.
- Storage equipment.
- Refinery residual fuel oil.
- Cat cracker feed.
- Reduced crude.
- Heavy feedstock.
- Pipeline with wax deposition.
Download PDF BETAFLOW 9800 Series - Dewaxing Agent
19. BETAFLOW 9841 - Anti Foulant
Fouling on gas compressors and process equipment can lower efficiency, raise energy consumption and increase pressure drop. It can also force a shutdown for cleaning. The fouling can come from organic material, inorganic material, corrosion products or solid matter carried along in the system.
BETAFLOW 9841 - Anti Foulant is a formulation of organic substances based on hydrocarbon. It is designed to prevent and minimise fouling on gas compressors. The product helps disperse solid matter so that it does not build up on the internal surfaces of the equipment.
Manfaat BETAFLOW 9841 antara lain:
- Helps prevent fouling on gas compressors.
- Helps disperse solid matter.
- Extends the interval between shutdowns.
- Helps keep equipment efficiency.
- Reduces the chance of organic, inorganic and corrosion product deposits building up.
Download PDF BETAFLOW 9841 - Anti Foulant
20. BETAFLOW 9850 Series - CO2 Removal Solvent
CO2 removal is an important part of gas treating. CO2 in a gas or liquid stream can lower product quality, increase the risk of corrosion and disturb the downstream process.
BETAFLOW 9850 Series - CO2 Removal Solvent is a formulated MDEA designed for the gas treating industry. The product helps remove CO2 from a gas or liquid stream selectively. It has the potential for a higher acid gas removal capacity than some conventional amines.
Aplikasi BETAFLOW 9850 Series antara lain:
- Natural gas treating.
- Coal gasification.
- Refinery system.
- Enhanced oil recovery.
- Tail gas treating.
- LPG treating.
- NGL treating.
- CO2 removal process.
The right solvent can help lower operating cost, reduce energy demand and increase the capacity of an existing system.
Download PDF BETAFLOW 9850 Series - CO2 Removal Solvent
21. BETAFLOW 9990 Series - Drag Reducing Agent
Pipeline crude oil usually faces flow problems from turbulent friction, high flow volume, deposits, paraffin or other restrictions in the pipeline. These conditions can raise back pressure and lower transport capacity.
BETAFLOW 9990 Series - Drag Reducing Agent is used to help reduce drag, lower back pressure and increase flow in crude oil pipelines. The product works by helping reduce turbulent friction in the flow system, so the energy needed to transport the fluid can go down.
Aplikasi BETAFLOW 9990 Series antara lain:
- Crude oil pipeline.
- Pipeline with restricted flow.
- Pipeline with high back pressure.
- Oil transport systems that need higher flow.
- Refinery and pipeline applications.
Manfaat drag reducing agent antara lain:
- Helps increase flow capacity.
- Helps lower back pressure.
- Reduces flow restriction from turbulence.
- Supports efficient crude oil transport.
- Helps optimise pipeline operation.
Download PDF BETAFLOW 9990 Series - Drag Reducing Agent
Tabel Ringkasan Produk Oilfield Chemicals BETAFLOW Series
| Produk | Fungsi Utama | Aplikasi |
|---|---|---|
| BETAFLOW 8080 Series | Antifoam / Defoamer | Separator, drilling, cementing, aqueous dan oil system |
| BETAFLOW 9120 Series | Corrosion Inhibitor OS | Produksi minyak, drilling, transportasi crude oil |
| BETAFLOW 9121 Series | Corrosion Inhibitor | Refinery, petrochemical, oilfield equipment |
| BETAFLOW 9121 WS | Water Soluble Corrosion Inhibitor | Water injection, produced water, hydrotest |
| BETAFLOW 9122 Series | Corrosion Inhibitor PF | Steam line, gas line, oil dan petrochemical plant |
| BETAFLOW 9123 Series | Corrosion Inhibitor OSWD | Oil production dan water injection |
| BETAFLOW 9130 Series | Scale Inhibitor | Water injection, produced water, pipeline |
| BETAFLOW 9131 Series | Chelating Agent | Stimulation, scale removal, cleaning surface facility |
| BETAFLOW 9140 Series | Oxygen Scavenger | Water injection dan hydrostatic test |
| BETAFLOW 9150 Series | H2S Scavenger | Sour gas, sour crude, produced fluid |
| BETAFLOW 9300 Series | Demulsifier | Separator, treater, crude oil dehydration |
| BETAFLOW 9310 Series | Deoiler / Reverse Demulsifier | Produced water dan refinery wastewater |
| BETAFLOW 9400 Series | Oil Spill Dispersant | Oil spill di air dan permukaan padat |
| BETAFLOW 9500 Series | Pour Point Depressant | Crude oil dengan wax/paraffin tinggi |
| BETAFLOW 9501 | Pour Point Depressant | Pipeline, storage tank, flowline |
| BETAFLOW 9600 Series | Biocide | Water injection, produced water, microbial control |
| BETAFLOW 9700 Series | TEG Formulated | Gas dehydration unit |
| BETAFLOW 9800 Series | Dewaxing Agent | Wax/paraffin control |
| BETAFLOW 9841 | Anti Foulant | Gas compressor dan process equipment |
| BETAFLOW 9850 Series | CO2 Removal Solvent | Gas treating dan CO2 removal |
| BETAFLOW 9990 Series | Drag Reducing Agent | Crude oil pipeline |
Manfaat Penggunaan Oilfield Chemicals yang Tepat
The right choice and application of oilfield chemicals can give several operational benefits, among them:
- Less downtime from corrosion, scaling, fouling and deposits.
- Longer life for pipes, separators, tanks, compressors and process equipment.
- Better oil and water separation.
- Produced water and refinery wastewater that stay within quality limits.
- Less risk of plugging from wax, paraffin or scale.
- Stable operation in gas treating and gas dehydration units.
- Better flow assurance in pipelines and production systems.
- Lower maintenance and operating costs over the long term.
- Safer operation in systems that contain H2S and acid gas.
- Energy savings in pipeline and gas treating systems.
Rekomendasi Pemilihan Oilfield Chemicals
Every oil and gas field has its own fluid characteristics, operating conditions, water composition, acid gas content, temperature, pressure and process problems. Therefore the choice of chemical treatment should not be based on the product name alone. It should come from a technical evaluation of the field conditions.
These are the factors to check before you choose oilfield chemicals:
- The main problem: corrosion, scale, foam, emulsion, wax, H2S, CO2, bacteria or fouling.
- Compatibility of the chemical with the process fluid and with the other chemicals already in use.
- The application method: continuous injection, batch treatment, slug dosing or direct injection.
- Temperature, pressure, pH, salinity and hydrocarbon content.
- Equipment material, type of dosing pump and injection point.
- The performance target, such as a lower corrosion rate, oil removal, water clarity or better flow.
- The monitoring and performance evaluation the chemical will need in the field.
Download PDF Technical Data Sheet Oilfield Chemicals
For more detail on each product in the BETAFLOW Series, please download the technical data sheet below:
- Download PDF BETAFLOW 8080 Series - Antifoam
- Download PDF BETAFLOW 9120 Series - Corrosion Inhibitor OS
- Download PDF BETAFLOW 9121 Series - Corrosion Inhibitor
- Download PDF BETAFLOW 9121 Series - Corrosion Inhibitor Water Soluble
- Download PDF BETAFLOW 9122 Series - Corrosion Inhibitor PF
- Download PDF BETAFLOW 9123 Series - Corrosion Inhibitor OSWD
- Download PDF BETAFLOW 9130 Series - Scale Inhibitor
- Download PDF BETAFLOW 9131 Series - Chelating Agent
- Download PDF BETAFLOW 9140 Series - Oxygen Scavenger
- Download PDF BETAFLOW 9150 Series - H2S Scavenger
- Download PDF BETAFLOW 9300 Series - Demulsifier
- Download PDF BETAFLOW 9310 Series - Deoiler Reverse Demulsifier
- Download PDF BETAFLOW 9400 Series - Oil Spill Dispersant
- Download PDF BETAFLOW 9500 Series - Pour Point Depressant
- Download PDF BETAFLOW 9501 - Pour Point Depressant
- Download PDF BETAFLOW 9600 Series - Biocide
- Download PDF BETAFLOW 9700 Series - TEG
- Download PDF BETAFLOW 9800 Series - Dewaxing Agent
- Download PDF BETAFLOW 9841 - Anti Foulant
- Download PDF BETAFLOW 9850 Series - CO2 Removal Solvent
- Download PDF BETAFLOW 9990 Series - Drag Reducing Agent
Kesimpulan
Oilfield chemicals play an important part in keeping oil and gas operations performing, safe and efficient. With the right chemical treatment, a company can control corrosion, scale, foam, emulsion, wax, fouling, bacteria, H2S, CO2 and flow restriction in pipelines.
PT Beta Pramesti Asia offers a range of chemicals for oilfield, refinery, gas treatment, produced water treatment, pipeline and supporting facilities in the oil and gas industry through the BETAFLOW Series.
For product consultation, chemical selection and field application recommendations, the technical team at Beta Pramesti Asia can help you choose the right chemical for your operating conditions.