Inside the HRSG: The High‑stakes Art of Finding Tube Failures Before They Find You

beta-pramesti-asiaindustry-power-generation-combinedprocess-ccgt

Inside the HRSG: The High‑stakes Art of Finding Tube Failures Before They Find You

Nearly half of HRSG tube failures hit the hot end. Proactive inspection and chemistry control can win back availability and cut costs. One plant learned this the hard way, with a ~50% steam-turbine derate.

Industry: Power_Generation_(Combined_Cycle_Gas_Turbine_ | Process: _CCGT)

The Heat Recovery Steam Generator (HRSG) is the boiler that turns gas-turbine exhaust into steam in a combined-cycle gas turbine plant (CCGT). It does not lead an easy life. The data says otherwise. Modern multi-pressure HRSGs, usually with reheat, are pushed hard in flexible, cycling duty, not just baseload. They accumulate damage in ways that surprise operators (tetra-eng.com) (tetra-eng.com).

Hot-end superheaters and reheaters are the bullseye. They account for nearly 50% of tube failures. Creep and fatigue drive ≈40% of failures, and multiple corrosion modes add ≈23%. Flow-accelerated corrosion (FAC) sits near 8% (tetra-eng.com) (tetra-eng.com).

The cost of neglect is real. Tube leaks trigger forced shutdowns and lost megawatts (tetra-eng.com). At CCPP Belawan in Indonesia, a 28-year-old HRSG had thinned tubes. They caused recurring leaks that forced the steam turbine to derate by ~50% and cut availability (researchgate.net).

Well-planned preventive programs work. Industry reviews put the penalty for poor maintenance at 5–20% lost capacity. Digital and predictive approaches can lift availability by ~5–15% and cut maintenance spend by ~18–25% (ncbi.nlm.nih.gov). GE adds that proactive HRSG upkeep reduces risk and improves reliability and availability. It catches corrosion, fouling, fatigue and creep early (gevernova.com) (gevernova.com).

Damage mechanisms and hot‑end exposure

Tetra Engineering's surveys show the dominant mechanisms and where they strike (Figure 1). High-temperature creep and fatigue cause ≈40% of tube failures. They are concentrated in superheater and reheater bundles and nearby headers under thermal cycling and high pressure. Corrosion causes ≈23% (tetra-eng.com) (tetra-eng.com). Corrosion includes under-deposit attack in economizers and stress-corrosion cracking at welds or lap joints. Ammonium bisulfate deposits (from SCR exhaust) and iron oxide are common culprits.

FAC (~8%) thins low‑alloy steels on the steam/water side under high velocity. However, after years of mitigation it is a smaller share than usually assumed (tetra-eng.com). Erosion and foreign object damage are rarer in gas‑fired units. However, gas‑path fins and tubes can still suffer if particulates or condensate are present. Mechanical overload and vibration can fatigue tube‑to‑header welds.

Hot-end steam sections (HP/IP superheaters and reheaters) see nearly half of failures. Therefore they need the closest surveillance (tetra-eng.com). No single inspection tool finds everything. Therefore multi-method NDT is mandatory.

Non‑destructive testing toolkit (NDT)

There is no one-size-fits-all NDT method. The choice depends on the materials and the defects (researchgate.net). Visual Testing (VT) uses borescopes and cameras to spot cracks, deposits and distortion through hand-holes and hatches. Even simple visual checks make the plant more reliable (tetra-eng.com) (tetra-eng.com). Surface replica techniques keep micro-crack evidence for later microscopy.

Ultrasonic Testing (UT) measures the remaining wall thickness in tubes, headers, drums and piping. Phased-array UT images welds. The Internal Rotary Inspection System (IRIS, an in-service rotating ultrasonic probe that uses a liquid couplant) gives full-circumference tube profiles. These profiles show localized pitting or erosion.

Eddy Current Testing (ECT) induces currents to flag wall loss and cracks. Remote-Field ECT (RFECT) suits carbon-steel tubing. Pulsed eddy current (PEC) systems such as Eddyfi Lyft can screen for inner-diameter corrosion from the outside, even over fins or insulation. They detect sub-2 mm defects and produce thickness maps with minimal disassembly (onestopndt.com). Operators use EC scanners to triage bundles quickly.

Magnetic Particle (MT) and Penetrant Testing (PT) find hairline surface cracks. MT is used on ferromagnetic parts and PT on non-ferrous parts. Both are standard for header and tube-end welds during shutdowns. Radiography (RT) with X-ray or gamma gives an image of thick welds and attachments when a joint is suspect.

Acoustic leak monitoring uses microphones to detect the high-frequency hiss of a steam leak in real time. Systems like Mistras AMS trend the signals and alarm when they pass a threshold. In the field they have flagged reheater and superheater leaks minutes before any plume was visible (ccj-online.com) (ccj-online.com).

Infrared thermography can show hot spots on casings and ducting. These hint at fouling or a leak inside. Laser profilometry and robotic crawlers with UT or EC probes check tight bends, returns and bowing of the whole bundle. Software matters too. Tools like Tetra's PipeVue collect and trend borescope images across outages for condition assessment (tetra-eng.com).

Inspection cadence and outage planning

Routine internal inspections are standard practice. Visual checks take place at every outage. Insurers or regulations usually need pressure‑boundary examinations for drums and headers. In the US, annual inspections are common (tetra-eng.com). Early‑life inspections set a baseline. Cycling and two‑shift units need more frequent looks, because cycling makes damage worse (tetra-eng.com) (tetra-eng.com).

During planned outages, full internal inspections (visual, UT, EC) cover economizers, evaporators, superheaters, reheaters, boiler drums and headers. Cleaning improves access for NDT. A professional chemical wash is usually scheduled together with an HRSG/boiler cleaning service to restore thermal performance.

A major overhaul every few years refreshes the asset: boiler washes, retubing the worst sections, and replacing attemperators or valve packs. At Belawan, tube replacement lifted the reliability factor by +0.137 (0–1 scale) and availability by +0.016. A financial analysis showed an IRR of ~7.5% and a positive NPV for full retubing (researchgate.net).

Online monitoring and performance flags

Continuous monitoring between outages catches drift early: vibration, temperatures, emissions and acoustic leak sensors. A rising gas-turbine back-pressure or an unexpected feedwater flow can point to economizer fouling. Then we check that area directly (gevernova.com). Analytics that track pressure-part tube thinning let operators time superheater/reheater repairs just ahead of a planned outage. That keeps steam output and avoids unplanned trips (gevernova.com) (ccj-online.com).

Chemistry control and deposit prevention

Water/steam chemistry is a front-line defense. A deviation in dissolved solids or corrosion products can signal FAC or under-deposit corrosion. Drain monitoring is a useful early indicator. Operators usually keep feedwater pH with a neutralizing amine program to limit carbonic acid attack in condensate return.

Removing dissolved oxygen is still important to prevent pitting. Oxygen scavenging is usually part of the regimen, with an oxygen scavenger matched to the operating pressure and temperature.

Stable alkalinity helps keep the protective magnetite layers in place. Boiler chemists usually standardize on an alkalinity control approach that matches the plant's AVT/OAVT philosophy.

Chemical precision matters. We handle metering with an accurate dosing pump so we avoid overfeed or underfeed, which can speed up corrosion or fouling.

Feedwater purity underpins all of this. Plants that use demineralized makeup usually put a demineralizer upstream of the HRSG to keep dissolved solids low. These solids drive under‑deposit attack.

To push silica and ionic impurities even lower, many facilities add a mixed‑bed polisher to achieve [less than 20 ppb silica](https://beta.co.id/en/blog/the-ppb-that-trips-a-turbine-inside-hrsg-steam-purity-separation-and-realtime-alarms) and very low total dissolved solids.

Some plants prefer continuous operation without chemical regeneration. For these, a continuous EDI system produces ultra-pure water and holds conductivity at boiler-grade levels.

Condensate return streams are usually cleaned with a [condensate polisher](https://beta.co.id/en/blog/the-hidden-workhorse-keeping-hrsgs-clean-condensate-polishing) to remove corrosion products before they deposit on economizer and evaporator tubes.

Risk‑based inspection and record‑keeping

Risk‑Based Inspection (RBI) turns inspection data into decisions. You track thickness readings, weld indications and defect locations over time. Then you can replace a tube just before it reaches the limit. Digital logs and trending tools help (onestopndt.com).

GE notes that HRSGs are usually serviced only when availability issues appear or at the annual. Therefore they stay suboptimal for long periods. A move to analytics‑driven inspections with smart sensors and AI keeps issues from growing into outages (gevernova.com) (gevernova.com) (ncbi.nlm.nih.gov).

NDT execution best practices

Focus on the high‑risk areas: gas‑path tubes and welds in superheater/reheater regions, and water/steam‑side high‑velocity circuits where FAC can bite. On the gas side, tube‑bundle faces usually show early stains or corrosion (tetra-eng.com).

Access and lighting decide the outcome. Scaffolds or manipulators bring cameras and probes within roughly 60 cm of the tube surfaces. High-intensity illumination and mirrors then reduce blind spots (tetra-eng.com).

Combine casing and tube checks. External casing and stack corrosion can hint at the conditions inside. Borescopes pay off on attemperators, burners and exhaust outlets.

Use more than one method to confirm an anomaly. Validate visual weld cracks with UT. Corroborate UT thinning with IRIS or PEC. Keep a database of thickness and defect trends so you can plan replacements (onestopndt.com).

Qualification matters. ASNT‑caliber training and careful interpretation improve accuracy. When we document findings and repairs, we build a knowledge base for RBI and budget cases. Early detection allows targeted work. We can clean the feedwater or treat it for silicate to stop economizer corrosion. We can add weld overlays or reinforce headers. This turns a “hidden” HRSG into a monitored asset (tetra-eng.com) (gevernova.com).

Preventive maintenance payback

Reliability and availability move in the right direction under proactive programs. At Belawan, retubing lifted reliability by 0.137 and availability by 0.016. Industry reviews put digital maintenance gains at ~5–15% availability improvement (researchgate.net) (ncbi.nlm.nih.gov).

Unplanned outages fall when leaks are found faster. Acoustic systems let operators repair days sooner than conventional detection. Therefore they avoid hours of forced downtime (ccj-online.com).

Costs go lower too. Optimized maintenance trims spend by roughly 20% in aggregated analyses. At Belawan, the tube replacement cost about IDR ~360 billion. It delivered positive NPV and ~7.5% IRR in its feasibility case (ncbi.nlm.nih.gov) (researchgate.net) (researchgate.net).

Performance retention follows naturally. Removing deposits and making timely repairs avoid rises in back‑pressure on the gas turbine that shave megawatts and erode cycle efficiency. A neglected HRSG can lose several efficiency points. Cleaning and replacement put that capacity back on line (gevernova.com).

Safety and compliance are reinforced, too. In many jurisdictions (and likely in Indonesia under boiler safety regulations), periodic internal pressure‑part inspections are mandatory. Preventive programs satisfy insurer and regulatory expectations and reduce catastrophic risk.

Industry trend lines and adoption

Risk‑based inspection models, condition monitoring, and asset‑management software are rising across combined‑cycle plants. HRSGs are also seeing more online acoustic leak detection and fiber‑optic RBI (Figure 2). Analysts put digital maintenance gains at material availability and cost improvements in new projects (ncbi.nlm.nih.gov). More aging HRSGs in Indonesia are reaching a condition that matters. Therefore systematic annual schedules and formal outage planning are expected to get more attention.

Bottom line: a good HRSG program blends fixed‑interval NDT, continuous monitoring, and timely repair. Plants that prioritize HRSG maintenance have fewer forced outages and hold higher availability than those that do not (tetra-eng.com) (gevernova.com). As one practitioner put it, the need to maintain the HRSG “is usually only realised in hindsight” after a tube failure trips the unit (tetra-eng.com).