WhatsApp

Article

The dirty secret of clean megawatts: why CCGT cooling water chemistry makes or breaks efficiency

beta-pramesti-asiaindustry-power-generation-combinedprocess-ccgt

In CCGT (combined‑cycle gas turbine) power plants, up to ~95% of intake water can be lost through evaporation. Therefore chemical control decides efficiency, cost and compliance. The key is a stable high COC (cycles of concentration), scale and corrosion inhibitors that work together, and a strong biocide program.

Open recirculating cooling systems in CCGT plants run under high heat loads with very large water volumes. Chemical discipline is the main line of defense. In industrial cooling tower systems, up to ~95% of makeup water can be lost as evaporation, and the rest is discharged as blowdown. COC (cycles of concentration) is the ratio of salt concentration in recirculating water to makeup water. If you raise COC, you reduce blowdown, and that directly cuts makeup water demand and effluent.

One clear example. A study of a 1,000-ton cooling tower showed that raising COC from 2.2 to 4.0 cut annual blowdown from ~8.08 million to ~3.23 million gallons (down −60%), and to ~1.08 million gallons at 10×COC (−85%). Indonesia's tropical climate is warm and humid, so scaling and biological growth get worse. Therefore this water conservation is increasingly important (www.mdpi.com).

The chemical program must also meet local regulations. For example, PerMenLH 08/2009 limits cooling tower blowdown to pH 6–9 with free Cl₂ ≤1.0 mg/L and PO₄³⁻ ≤10 mg/L (www.scribd.com). Therefore you need a balanced high-COC program. It must protect heat transfer, suppress scaling and corrosion, control biofouling, and meet effluent quality standards.

Scale-control regime and inhibitors

Mineral scale (CaCO₃, CaSO₄, Ca₃(PO₄)₂, silica) quickly insulates heat exchanger surfaces and reduces efficiency. These salts tend to deposit on hot surfaces (retrograde solubility) or at locations with high local pH, such as cathodic sites. The simplest operation is to keep the bulk water unsaturated (low COC or acid injection). However, this uses a lot of water.

Modern practice has moved to threshold inhibitors that allow high COC without scaling. Commercial programs combine organic phosphonates and dispersant/growth-inhibitor polymers:

- Secondary phosphonates (organophosphorus inhibitors such as HEDP, ATMP, NTMP) adsorb onto newly formed crystals. They stop nucleation and crystal growth, and they chelate Ca²⁺/Fe²⁺. Typical doses are only a few ppm, about 2–10 mg/L as PO₄ equivalent. At these doses they inhibit scale well without stoichiometric dosing. By contrast, chelants such as EDTA need almost a 1:1 dose with Ca. That is difficult for hard water.

- Dispersant polymers and growth inhibitors (for example polyacrylates, polyvinyl phosphonic acids, maleic/LAS polymers) keep crystals suspended. In the field, phosphonates and polymers are blended to target CaCO₃, CaSO₄, silica, and others. This is the same as the usual package of industrial cooling tower chemical program, scale inhibitors for cooling tower, and dispersant.

Performance evidence: a combination of flexible polymers and crystal growth inhibitors keeps heat exchanger tubes “essentially free” of corrosion and deposits after program conversion. A high-COC strategy that also uses softened makeup water reduced the CaCO₃ formation rate to nearly zero in trials. Silica is difficult because conventional inhibitors affect it less. In these cases periodic acid cleaning or RO pretreatment is sometimes needed. Options such as Brackish Water RO can serve as pretreatment.

Phosphate and silica note: phosphate in circulation can accumulate. Environmental limits (for example 10 mg/L in Indonesia) restrict phosphate addition (www.scribd.com). Therefore modern programs usually limit orthophosphate and rely on polymer modifiers.

Outcome: a maintained tower can run at 4–8× COC without fouling. Systems without protection are usually limited to 2–3×. For Indonesian conditions (high hardness/humidity), this means avoiding repeated cleaning and outages. In makeup water, softening with a softener is usually used to push COC higher.

Multi-metal corrosion inhibition strategy

Cooling loop materials in CCGTs are usually mixed: carbon steel piping, stainless or cupronickel condenser tubes, and brass/admiralty in tower sections. A good program combines pH control and inhibitors to protect all surfaces at once. This follows the corrosion inhibitors package for cooling tower applications.

- pH control (~8–8.5): most open recirculating systems run at slightly alkaline pH to suppress general corrosion. At pH ~8.2, a thin CaCO₃ film usually forms and passivates steel. Corrosion rate rises sharply below pH 7 or above ~9. Alkalinity is maintained (for example with caustic or amine) so pH stays in the upper-7 to mid-8 range without driving heavy scaling. A neutralizing amine is one option, such as neutralizing amine.

- Anodic inhibitors (nitrite, molybdate): for ferrous circuits, nitrite (NaNO₂) at hundreds of ppm is the standard. The industry maintains ~500–1,000 mg/L nitrite for full passivation of steel, with steel corrosion rates falling below ~0.5 mpy (mils per year, 1 mil = 0.001 inch). Molybdate is an alternative at ~1/3 the nitrite dose. Both need a little dissolved oxygen to form a protective oxide. Nitrite can trigger nitrifying bacteria and nitrosamine formation with amines, so an oxidizer and/or alternative chemicals are used alongside.

- Cathodic/filming inhibitors (amine, phosphate, silicate): some programs add phosphate or silicate as a cathodic inhibitor, but environmental effluent issues limit this. Some plants use filming amines (for example octadecylamine or morpholine) to coat steel. This also helps with pH control. Modern non-phosphate polymeric programs usually include proprietary filming agents and silicate.

- Copper/aluminum protection: copper/brass alloys need passivation with an azole (benzotriazole/tolyltriazole) that adsorbs and forms a passive film. If the dose is maintained, copper corrosion is almost zero. Lab coupons show <0.2 mpy in well-treated systems. Note: chlorination and some treatments consume azole, so the dose must be maintained. Alternative oxidizers such as chloramines or ClO₂ are sometimes chosen to avoid rapid film degradation.

- Heavy metal restrictions: older programs used Zn or chromate, which are now banned. Indonesian regulations prohibit Zn and Cr(VI), and even Cu discharge is tightly limited (www.scribd.com). Therefore modern chemistry avoids soluble Zn or chromate. The trend is toward non-phosphate/non-zinc polymer programs.

Outcome: at 10×COC with optimized chemistry, steel corrosion is ~0.25–0.5 mpy and copper alloy corrosion is ~0.01 mpy. In practice, condenser loops that are maintained well usually show coupons ≤0.5 mpy. Monitoring dissolved iron/copper and pH confirms passive conditions. Keeping [Cl⁻] well below the pitting threshold is also standard. A complete cooling tower chemical package and precise dosing with a dosing pump help achieve this consistency.

Biological control and biofilm management

Cooling towers are an ideal habitat for microorganisms. Biofilm that forms in the fill and heat exchangers can cut heat transfer drastically, even by up to half, and trigger Legionella (www.mdpi.com). Scale and biofilm work together. Deposits protect bacteria and Legionella, and "stagnation, biofilm and scale enhance Legionella survival and multiplication" (www.mdpi.com). Therefore scale control is part of microbiological control. CDC emphasizes that "scale, corrosion, sediment controls, and system cleaning are important" for [Legionella prevention](https://beta.co.id/en/blog/a-tropical-perfect-storm-inside-the-palm-oil-industrys-cooling-tower-plan-to-beat-legionella) (www.cdc.gov).

Oxidizers: chlorine (gas/NaOCl/HOCl), bromine, chlorine dioxide (ClO₂), or ozone are usually used. In practice, an oxidizer residual is maintained in the basin (for example 0.2–0.5 mg/L free Cl₂) plus periodic higher-dose “shock”. Studies show that continuous chlorination alone is not sufficient (www.mdpi.com). However, the addition of periodic hyper‑chlorination reduces Legionella by 1–2 log (p<0.05) (www.mdpi.com). Guidelines (CDC/ASHRAE/etc.) recommend continuous feed via a metering pump and a shock schedule (www.mdpi.com) (www.cdc.gov). ClO₂ is usually selected in high-flow systems because it produces fewer stable chlorides and a longer residual (www.mdpi.com). For a safe and stable chlorine supply, the electrochlorination option (making NaOCl from brine) is operationally relevant.

Non-oxidizers: aldehydes (for example glutaraldehyde), isothiazolinone, guanidine, THPS, and others work more slowly but can penetrate thick biofilm and are not neutralized by organic load. Common strategy: continuous oxidizer (low dose) plus 2–3 weekly pulses of non-oxidizer (for example 5–20 mg/L glutaraldehyde). THPS is usually used at a 3–5 mg/L release, or DBNPA at ~5 mg/L based on product technical documentation. Non-oxidizers are important when chlorine alone fails, as in the illustration of H₂O₂/Ag failure in one test (www.mdpi.com). The right biocides package, combined with continuous feed using a dosing pump, provides broad-spectrum control.

Monitoring covers HPC (heterotrophic plate count) and Legionella specifically. The CDC practice target is HPC <10⁴ CFU/mL and Legionella not detected. Disinfectant residual is tracked (free Cl₂ or ORP/oxidation-reduction potential). Many plants dechlorinate blowdown or switch to ClO₂ to support chemical control and effluent compliance (free Cl₂ ≤1.0 mg/L) (www.scribd.com). Products such as dechlorination agent, UV sterilizers such as ultraviolet, or filtration help reduce chemical consumption and support compliance.

An effective biocide regimen drastically reduces microbial fouling. The same study recorded Legionella falling from ~10⁶ to ~10³ CFU/L with a shock/continuous combination (www.mdpi.com). A well-maintained tower shows no visible slime. Its HPC is several times lower than without treatment.

Integrated program and performance indicators

- COC: we monitor COC via conductivity or TDS. The target is ≥4–6× COC with stable chemistry. Increasing COC from ~2×→4× has been shown to cut blowdown by about half. Regular blowdown testing keeps mineral accumulation below the saturation margin. Pretreatment of suspended solids with media such as sand/silica filter helps keep the circuit clean.

- Corrosion: coupons or electrical probes are installed in the condenser loop. Typical targets are ≤1 mpy for steel and undetected copper loss. If it rises (>1 mpy steel), inhibitor dose is adjusted. On-spec industrial operations usually record 0.2–0.5 mpy.

- Scale: regular inspection of pump strainers, heat exchanger delta‑T, or rising pressure drop gives an early warning. Ideally, mechanical cleaning is no more than annual. With a crystal growth inhibitor program, deposit cleaning intervals can stretch to 6–12 months. industrial cooling tower cleaning services help schedule them. The right strainer device adds visibility into field conditions.

- Microbiology: measure weekly or monthly. After a program change, target a one-order-of-magnitude reduction. For example, a Legionella target below 50 CFU/L in recirculating water, and HPC in the thousands per mL range or lower under treatment. Control charts give assurance of microbiological health.

- Cost and compliance: every improvement in condenser pressure (kPa/bar) or drop in cooling water temperature (°C) lowers heat rate and increases output at multi-hundred-MW plants. Preventing scale and keeping the condenser clean maintains BFW purity, so performance stays at design. Data-based outcomes: 60% blowdown reduction, fouling reduction >80%, steel corrosion <0.5 mpy, and Legionella reduction >90%. Compliance with PerMenLH 08/2009 is mandatory. For example, phosphate and heavy metals must stay below the thresholds (www.scribd.com).

- Industry trends: utilities are moving to digital monitoring (online sensors for ORP, conductivity, microbiology). Monitoring Cooling Tower Sentinel CTS can support this. Non-phosphate chemistries and biofilm inhibitor blends are increasingly preferred over older methods. For challenging makeup (hardness/silica), membrane options such as nano-filtration or membrane systems packages can be considered as pretreatment toward high COC.

Technical and compliance summary

[Coordinated chemical program](https://beta.co.id/blog/menjinakkan-menara-pendingin-pabrik-sawit-resep-kimia-terkoordinasi-untuk-panas-tinggi-dan-air-kaya-organik) with threshold inhibitors (phosphonate/polymer), corrosion passivators (nitrite/molybdate/azole) and strong biocides is the “insurance” for large-capacity CCGT cooling systems. Data and field practice show that such a program can cut blowdown, practically eliminate scale, hold corrosion at sub-mpy, and suppress Legionella >90% (www.mdpi.com). In Indonesia, this evidence-based approach improves efficiency and reliability, and it keeps the effluent within the limits, for example chloride and phosphate (www.scribd.com).