Water and waste water chemical
Anionic vs Cationic Flocculants
Updated
BETAGARD anionic vs cationic flocculants for clarification, thickening, and dewatering, selected by solids, charge, shear, make-down, dose, and plant trials.
Discuss the application.
Send the application, operating conditions and the result you expect. Our team will discuss the options with you.
Choose an anionic or cationic flocculant from the solids and the water, not from a simple “opposite charge” rule. Operators should screen grades at bench scale. Then prove make-down, dose, injection point, floc strength, overflow or filtrate quality, sludge or cake, consumption and cost in a controlled plant trial.
PT Beta Pramesti Asia, through beta.co.id, supplies BETAGARD polymer flocculants for clarification, thickening, filtration aid and dewatering in Indonesia. This page lists several anionic and cationic grades. The TDS, SDS, batch and application test govern the final grade and use limits.
Technically reviewed: 31 July 2026.
When should an anionic or cationic flocculant be shortlisted?
Ionic charge helps form a shortlist. However, performance also depends on charge density, molecular weight, product form, pH, salinity, temperature, solids type, coagulant, mixing energy, shear and the separation unit. Compare candidates on the same sample and procedure.
| Selection question | Anionic candidates are often screened when | Cationic candidates are often screened when | Deciding evidence |
|---|---|---|---|
| What is the process duty? | Mineral clarification, thickening, filtration aid, or solids responding to anionic bridging | Organic-sludge conditioning or streams responding to cationic polymer | Blank/control and a screen across charge densities |
| What are the solids? | Mineral solids or surfaces showing a good test response | Organic/biological sludge or surfaces showing a good test response | Zeta/charge test where available, pH, TSS, volatile solids, oil, and floc observation |
| What constrains the unit? | Shear, settling, recycle, filter, and carryover | Shear, drainage, cake release, filtrate, and downstream effect | Test at representative mixing, contact time, and equipment |
| What are the chemical risks? | Overdose, residual polymer, slippery spills, lumps, and poor make-down | The same risks plus effects on biological or filtrate systems | Dose sweep, SDS/TDS, compatibility, and acceptance criteria |
This table is a screening framework. It is not a rule that one charge always fits one industry. The U.S. Bureau of Reclamation identifies polymer type, purpose and testing as the basis for demand. The U.S. EPA dewatering manual also connects conditioning decisions to tests, equipment, handling, sludge volume, performance and cost.
Which evidence is required before releasing a grade?
| Stage | Minimum evidence | Decision |
|---|---|---|
| Product | Name/grade, powder or emulsion form, charge, batch, TDS/SDS, shelf life, and package condition | Match material to the approved trial |
| Make-down | Dilution water, concentration, wetting sequence, mixing energy, hydration/maturation time, solution age, and lumps | Release, hold, or remake the solution |
| Dosing | Pump output at backpressure, dose basis, flow/dry solids, injection point, dilution, interlock, and consumption | Establish delivered rate, not just a setpoint |
| Response | Overflow/filtrate, settling/drainage, floc size and strength, blanket, cake solids, capture, and downstream effect | Accept a range, correct one variable, or reject |
| Commercial | Product use, make-down water, supporting chemicals, sludge, energy, downtime, and handling | Compare total cost per unit of water or solids |
For cross-family screening, review industrial flocculants, PAC and ACH coagulants, and sludge-treatment programmes. Watermart dosing-pump capacity and materials should match the actual solution, pressure, and flow.
Flocculant-selection FAQs
Is a cationic flocculant always used for biological sludge?
Not always. It is a common screening point, not the final decision. Sludge source, surface charge, pH, salinity, oil, coagulant, shear, dewatering unit, filtrate and downstream limits still have to be tested.
Is the highest-molecular-weight grade the most effective?
Not automatically. Molecular weight and charge density affect bridging, wetting, viscosity, shear sensitivity and feed. However, the result comes from the combination of product, make-down, mixing, injection point, solids and equipment.
Which data should be sent for a shortlist?
Send water or sludge source, flow or dry-solids rate, pH, TSS and volatile solids, oil/organics, salinity, coagulant, separation unit, bench-test results, make-down, pump, overflow/filtrate/cake quality and the operating problem through the PT Beta Pramesti Asia contact page.
Betagard Anionic and Cationic Oil Based Polymeric Flocculants
BETAGARD 6100
Anionic Flocculant
BETAGARD 6100 is an anionic polyelectrolyte. It works as a coagulant aid or sludge conditioning agent in liquid-solids separation. This product is an anionic polymer with a high charge, and it works as a flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable where the flocks formed are subject to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%. Its residual monomer content is low, so BETAGARD 6100 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Anionic | Very High | BETAGARD 6100 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6100 should be stored in a dry place with an ambient temperature of not more than 38o C. Tightly close the drum container after use. | Available in plastic container sizes of 15 kgs or PE bags up to 25 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6100 for different applications is as follows:
- Flocculant: 0.1 to 2.0 ppm
- Coagulant Aid: 0.05 to 1.0 ppm
- Filtration Aid: 0.01 to 1.0 ppm
- Sludge Dewatering: 0.5 to 4.0 kg per ton of dry solids
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less before you add it to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.
BETAGARD 6100 Series
RO & UF ANTISCALANT and WETTED SURFACE AIR COOLER SCALE INHOBITOR
Betagard 6100 Series is a multifunctional antiscalant and antifoulant for reverse osmosis systems. It is very effective in controlling crystallization and particulate fouling on membrane surfaces.
Betagard 6100 will control the scale deposition of CaCO3, CaSO4, BaSO4, and CaF2. Betagard 6100 is formulated to control soluble and insoluble iron and actively disperse particulates. Hydro 600 is effective against silica fouling. It is specifically designed for use on Thin Film and CA membranes.
Technical Specifications
| Physical Form | pH | Sp. Gravity at 25 DEG C | Handling and Storage Measures | Packaging |
|---|---|---|---|---|
| Colorless clear colored liquid. | 5.0 - 6.0 | Anionic | Keep out of reach of children. In case of accidental splashing, flush with plenty of water. And for eye contact, must receive medical attention as a safety measure. | Available in plastic container size with a net weight of 200 liters / drum. |
Dosage & Usage Instructions:
Betagard 6100 is an aqueous solution of organic acids. It is corrosive in concentrated form. Therefore you need dosing equipment that resists corrosion. Suitable materials are 316L stainless steel or plastics such as GRP, PVC and PE. The recommended injection point is into the feed water, downstream of filtration equipment and cartridge filters. Betagard 6100 mixes with water in all proportions.
It can be applied as a neat product, or as a solution in distillate. We recommend a minimum solution strength of 10% w/b. Betagard 6100 should be dosed continuously and in proportion to the feed water flow, to keep the recommended dosing rate. The dosage rate you need depends on the feed water quality and the saturation index of the scale forming species present in the concentrated brine. The usual dosage rate range is between 5 and 15 ppm.
BETAGARD 6110
Anionic Flocculant
BETAGARD 6110 is an anionic polyelectrolyte. It serves as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is a very charged anionic polymer, which will serve as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are usually prepared at concentrations of 0.1 to 0.5%. Due to its low residual monomer content, BETAGARD 6110 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Anionic | Very High | BETAGARD 6110 solution is essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6110 should be stored in a dry place with an ambient temperature of no more than 38oC. Tightly close the drum container after use. | Available in fiber drum or PE bag size - 25 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6110 for different applications is as follows:
- Flocculant: 0.1 to 2.0 ppm
- Coagulant Aid: 0.05 to 1.0 ppm
- Filtration Aid: 0.01 to 1.0 ppm
- Sludge Dewatering: 0.5 to 4.0 kg per ton of dry solids
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. These stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, dilute the stock solution further with clean water to 0.02% or less before you add it to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.
BETAGARD 6120
Anionic Flocculant
BETAGARD 6120 is an anionic polyelectrolyte. It works as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is an anionic polymer with a high charge, and it works as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are usually prepared at concentrations of 0.1 to 0.5%. Because its residual monomer content is low, BETAGARD 6120 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Anionic | Very High | BETAGARD 6120 solutions are essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6120 should be stored in a dry place with an ambient temperature of no more than 38oC. Tightly close the drum container after use. | Available in fiber drum or PE bag size - 25 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6120 for different applications is as follows:
- Flocculant: 0.1 to 2.0 ppm
- Coagulant Aid: 0.05 to 1.0 ppm
- Filtration Aid: 0.01 to 1.0 ppm
- Sludge Dewatering: 0.5 to 4.0 kg per ton of dry solids
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. These stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, dilute the stock solution further with clean water to 0.02% or less before you add it to the process stream. However, this is usually determined by inspection of available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.
BETAGARD 6130
Anionic Flocculant
BETAGARD 6130 is an anionic polyelectrolyte. It works as a coagulant aid or sludge conditioning agent in liquid-solids separation. This product is an anionic polymer with a high charge, so it works well as a flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable where the flocks formed are subject to high shear. Stock solutions are usually prepared at concentrations of 0.1 to 0.5%. Its residual monomer content is low, so BETAGARD 6130 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Anionic | Very High | BETAGARD 6130 solutions are essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6130 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use. | Available in fiber drum or PE bag size - 25 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6130 for different applications is as follows:
- Flocculant: 0.1 to 2.0 ppm
- Coagulant Aid: 0.05 to 1.0 ppm
- Filtration Aid: 0.01 to 1.0 ppm
- Sludge Dewatering: 0.5 to 4.0 kg per ton of dry solids
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less before it goes into the process stream. However, this is usually determined by inspection of the available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.
BETAGARD 6140
Anionic Flocculant
BETAGARD 6140 is an anionic polyelectrolyte. It works as a coagulant aid or sludge conditioning agent in liquid-solids separation. This product is an anionic polymer with a high charge, so it works well as a flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable where the flocks formed are subject to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%. Its residual monomer content is low, so BETAGARD 6140 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Anionic | Very High | BETAGARD 6140 solutions are essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6140 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use. | Available in fiber drum or PE bag size - 25 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6140 for different applications is as follows:
- Flocculant: 0.1 to 2.0 ppm
- Coagulant Aid: 0.05 to 1.0 ppm
- Filtration Aid: 0.01 to 1.0 ppm
- Sludge Dewatering: 0.5 to 4.0 kg per ton of dry solids
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. These stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, dilute the stock solution further with clean water to 0.02% or less before it goes into the process stream. However, this is usually determined by inspection of the available facilities. The recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.
BETAGARD 6150
Anionic Flocculant
BETAGARD 6150 is an anionic polyelectrolyte. It serves as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is an anionic polymer with a high charge, and it works as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%. Its residual monomer content is low, so BETAGARD 6150 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Anionic | Very High | BETAGARD 6150 solutions are essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6150 should be stored in a dry place with an ambient temperature of no more than 38oC. Close the drum container tightly after use. | Available in plastic drum size 15 kgs or PE bag - 25 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6150 for different applications is as follows:
- Flocculant: 0.2 to 2.0 ppm
- Coagulant Aid: 0.1 to 1.0 ppm
- Filtration Aid: 0.02 to 1.0 ppm
- Sludge Dewatering: 0.5 to 4.0 kg per ton of dry solids
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. These stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, dilute the stock solution further with clean water to 0.02% or less before you add it to the process stream. However, this is usually determined by inspection of the available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.
BETAGARD 6160
Anionic Flocculant
BETAGARD 6160 is an anionic polyelectrolyte. It works as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is an anionic polymer with a high charge, and it works as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable for applications where the flocks formed are subject to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%. Because it has a low residual monomer content, BETAGARD 6160 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Anionic | Very High | BETAGARD 6160 solutions are essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6160 should be stored in a dry place with an ambient temperature of no more than 38oC. Close the drum container tightly after use. | Available in plastic drum size 15 kgs or PE bag - 25 kgs. |
Dosage & Usage Instructions:
We recommend the following dosage of BETAGARD 6160 for different applications:
- Flocculant: 0.2 to 2.0 ppm
- Coagulant Aid: 0.1 to 1.0 ppm
- Filtration Aid: 0.02 to 1.0 ppm
- Sludge Dewatering: 1.0 to 4.0 kg per ton of dry solids
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high-speed, high-shear mechanical mixers for stirring. These stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, dilute the stock solution further with clean water to 0.02% or less before you add it to the process stream. However, this is usually determined by inspection of the available facilities. Recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.
BETAGARD 6170
Anionic Flocculant
BETAGARD 6170 is an anionic polyelectrolyte. It works as a coagulant aid or sludge conditioning agent in liquid-solids separation. This product is a very charged anionic polymer. It works as an effective flocculant in many liquid/solids separation systems, including clarification, thickening and dewatering. This product is suitable where the flocks formed are subject to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%. Its residual monomer content is low, so BETAGARD 6170 can be used in drinking water treatment up to a maximum concentration of 1.0 mg/l, as approved by the Indonesian Ministry of Health.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Anionic | Very High | BETAGARD 6170 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6170 should be stored in a dry place with an ambient temperature of no more than 38oC. Tightly close the drum container after use. | Available in fiber drum or PE bag size - 15 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6170 for different applications is as follows:
- Flocculant: 0.2 to 2.0 ppm
- Coagulant Aid: 0.1 to 1.0 ppm
- Filtration Aid: 0.02 to 1.0 ppm
- Sludge Dewatering: 1.0 to 4.0 kg per ton of dry solids
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high-speed, high-shear mechanical mixers for stirring. Such stock solutions are stable for at least 3 days. Refer to the polymer mixing procedure bulletin. For best performance, further dilute the stock solution with clean water to 0.02% or less before you add it to the process stream. However, this is usually determined by inspection of the available facilities. The recommended transfer pumps are gear type or positive displacement piston or diaphragm pumps.
BETAGARD 6200
Cationic Flocculant
BETAGARD 6200 is a cationic polyelectrolyte. It works as a coagulant aid or a sludge conditioning agent in liquid-solids separation. This product is used mainly for wastewater purification, and also for thickening and dewatering municipal and industrial sewage sludge (centrifuges, belt filter presses, chamber filter presses). This product is particularly suitable where the formed flocks are subject to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Cationic | Very High | BETAGARD 6200 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6200 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use. | Available in fiber drum or PE bag size - 15 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6200 for different applications is as follows:
- Clarification of secondary effluent: 1 to 5 ppm.
- Flocculation, thickening and dewatering of primary and secondary sludge from municipal sewage and from several industries: 0.5 to 4.0 kg per ton of dry solids.
- Centrifugal operation: 1.5 to 5.0 kg per ton of dry solids.
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for agitating. This stock solution is stable for at least two days. Its charge density does not change much in that time, so its performance results stay the same. To make sure the solution stays stable, use water with a temperature lower than 40oC for dissolution. The pH of the solution should be kept within the range of 5.0 to 6.5. For best performance, dilute the stock solution further with clean water to 0.02% to 0.03% or less before feeding it to the process stream. Dilution can be done using in-line dilution or by using a dilution tank. However, this is usually determined by inspection of the facilities available. The recommended transfer pumps are gear type piston pumps or positive displacement piston pumps.
BETAGARD 6210
Cationic Flocculant
BETAGARD 6210 is a cationic polyelectrolyte. It works as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is used primarily for wastewater purification, and also for thickening and dewatering municipal and industrial sewage sludge (centrifuges, belt filter presses, chamber filter presses). This product is particularly suitable for applications where the formed flocks are subjected to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Cationic | Very High | BETAGARD 6210 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6210 should be stored in a dry place with ambient temperature not more than 38oC. Tightly close the drum container after use. | Available in fiber drum or PE bag size - 25 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6210 for different applications is as follows:
- Clarification of secondary effluent: 1 to 5 ppm.
- Flocculation, thickening and dewatering of primary and secondary sludge from municipal sewage and from several industries: 0.5 to 4.0 kg per ton of dry solids.
- Centrifugal operation: 1.5 to 5.0 kg per ton of dry solids.
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for agitating. This stock solution is stable for at least two days without significant changes in its charge density that could affect its performance results. To keep the solution stable, use water with a temperature lower than 40oCfor dissolution. The pH of the solution should be controlled within the range of 5.0 - 6.5. For best performance, dilute the stock solution further with clean water to 0.02% - 0.03% or less before feeding it to the process stream. Dilution can be done using in-line dilution or by using a dilution tank. However, this is usually determined by inspection of the facilities available. The recommended transfer pumps are gear type piston pumps or positive displacement piston pumps.
BETAGARD 6220
Cationic Flocculant
BETAGARD 6220 is a cationic polyelectrolyte. It works as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is used primarily for wastewater purification, as well as for thickening and dewatering municipal and industrial sewage sludge (centrifuges, belt filter presses, chamber filter presses). This product is particularly suitable for applications where the formed flocks are subjected to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Cationic | Very High | BETAGARD 6220 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6220 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use. | Available in fiber drum or PE bag size - 25 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6220 for different applications is as follows:
- Clarification of secondary effluent: 1 to 5 ppm.
- Flocculation, thickening, and dewatering of primary and secondary sludge of municipal sewage and of several industries: 0.5 to 4.0 kg per ton of dry solids.
- Centrifugal operation: 1.5 to 5.0 kg per ton of dry solids.
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for stirring. This stock solution is stable for at least two days without significant changes in its charge density that could affect its performance results. To keep the solution stable, use water with a temperature lower than 40oCfor dissolution. Also keep the pH of the solution within the range of 5.0 - 6.5. For best performance, dilute the stock solution further with clean water to 0.02% - 0.03% or less before feeding it to the process stream. Dilution can be done using in-line dilution or by using a dilution tank. However, this is usually determined by inspection of the facilities available. The recommended transfer pumps are gear type piston pumps or positive displacement piston pumps.
BETAGARD 6230
Cationic Flocculant
BETAGARD 6230 is a cationic polyelectrolyte. It works as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is used mainly for wastewater purification, and also for thickening and dewatering municipal and industrial sewage sludge (centrifuges, belt filter presses, chamber filter presses). This product is particularly suitable for applications where the formed flocks are subjected to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Cationic | Very High | BETAGARD 6230 solution is essentially non-corrosive. Recommended construction materials for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6230 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use. | Available in fiber drum or PE bag size - 25 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6230 for different applications is as follows:
- Clarification of secondary effluent: 1 to 5 ppm.
- Flocculation, thickening, and dewatering of primary and secondary sludge of municipal sewage and of several industries: 0.5 to 4.0 kg per ton of dry solids.
- Centrifugal operation: 1.5 to 5.0 kg per ton of dry solids.
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for agitating. This stock solution is stable for at least two days without significant changes in its charge density that could affect its performance results. To keep the solution stable, use water with a temperature lower than 40oCfor dissolution. The pH of the solution should be controlled within the range of 5.0 to 6.5. For best performance, dilute the stock solution further with clean water to 0.02% to 0.03% or less before feeding it to the process stream. Dilution can be done using in-line dilution or by using a dilution tank. However, this is usually determined by inspection of the facilities available. The recommended transfer pumps are gear type piston pumps or positive displacement piston pumps.
BETAGARD 6240
Cationic Flocculant
BETAGARD 6240 is a cationic polyelectrolyte. It works as a coagulant aid or sludge conditioning agent in liquid-solids separation processes. This product is used primarily for wastewater purification, as well as for thickening and dewatering municipal and industrial sewage sludge (centrifuges, belt filter presses, chamber filter presses). This product is particularly suitable for applications where the formed flocks are subjected to high shear. Stock solutions are usually prepared at a concentration of 0.1 to 0.5%.
Technical Specifications
| Physical Form | Bulk Density, gr/ml | Ionic Charge | Molecular Weight | Handling and Storage Measures | Packaging |
|---|---|---|---|---|---|
| Off white colored powder. | 0.65 - 0.90 | Cationic | Very High | BETAGARD 6240 solution is essentially non-corrosive. Recommended materials of construction for solution handling include black iron, mild steel, fiber glass, plastics, and other more resistant materials. Galvanized equipment should not be used. Spilled polymer is very slippery. Spilled polymer should be scooped up and wiped off before rinsing with water. BETAGARD 6240 should be stored in a dry place with an ambient temperature of not more than 38oC. Tightly close the drum container after use. | Available in fiber drum or PE bag size - 25 kgs. |
Dosage & Usage Instructions:
The recommended dosage of BETAGARD 6240 for different applications is as follows:
- Clarification of secondary effluent: 1 to 5 ppm.
- Flocculation, thickening, and dewatering of primary and secondary sludge of municipal sewage and of several industries: 0.5 to 4.0 kg per ton of dry solids.
- Centrifugal operation: 1.5 to 5.0 kg per ton of dry solids.
The actual dosage should be determined in a laboratory tube test. Stock solutions are usually made to a concentration of 0.1 to 0.5%. Do not use high speed, high shear mechanical mixers for agitating. This stock solution is stable for at least two days without significant changes in its charge density that could affect its performance results. To keep the solution stable, use water with a temperature lower than 40oCfor dissolution. The pH of the solution should be kept in the range of 5.0 - 6.5. For best performance, dilute the stock solution further with clean water to 0.02% - 0.03% or less before feeding it to the process stream. Dilution can be done with in-line dilution or with a dilution tank. However, this is usually determined by inspection of the facilities available. The recommended transfer pumps are gear type piston pumps or positive displacement piston pumps.
Contact Us
Want to know more about BETAGARD Anionic and Cationic Oil Based Polymeric Flocculants? Contact us now for more information or for technical consultation about the application of this product in your water treatment system.