Poly aluminium chloride (PAC)
Liquid PAC for Drinking Water: Trial Guide
Updated
Select liquid PAC for drinking water from lot specifications, active basis, basicity, impurities, jar tests, aluminium residual, sludge, and dosing proof.
Discuss the application.
Send the application, operating conditions and the result you expect. Our team will discuss the options with you.
Liquid PAC for drinking water is a candidate coagulant. It is not proof that the water is immediately safe to drink. Before routine use, a plant should check the grade and the lot, the active basis, basicity, impurities, the pH response, jar tests on the source water, aluminium residual, sludge production, the calibrated dose, and how the downstream filtration and disinfection perform.
PT Beta Pramesti Asia, through beta.co.id, supplies liquid PAC and helps with coagulation reviews for drinking-water and process-water plants in Indonesia. Product, dose and acceptance criteria still depend on the lot documents, the test results, the downstream treatment and the finished-water requirements that apply.
Last technically reviewed: 2 August 2026.
What does liquid PAC for drinking-water treatment mean?
PAC, or polyaluminium chloride, destabilises colloidal particles so that floc can be separated by sedimentation or DAF and filtration. Procurement specifications must define what the “drinking” label means. A trade name is not automatic evidence that a particular lot suits the plant and the source water.
SNI 3822:2018 Polialuminium klorida was listed as current on 2 August 2026. It covers quality requirements and test methods for liquid and solid PAC used as a water-clarification chemical. That product standard is not an operating dose and does not replace finished-water verification.
Indonesia Ministry of Health Regulation No. 2 of 2023 was listed as current on 2 August 2026. It provides the environmental-health requirements framework, including drinking water. Each facility should confirm the schedules that apply, the surveillance requirements, the permits, the customer specifications and any later amendments.
What data determine liquid PAC selection?
An auditable choice connects product identity with the source-water response. Price per kilogram and dose in mg/L are not comparable unless active content, density, pH and alkalinity demand, sludge volume and finished-water quality share a common basis.
| Procurement or process input | Minimum evidence | Decision supported |
|---|---|---|
| Product and lot identity | Product name, grade, lot, manufacturer, production date, TDS, SDS, and the delivered lot’s Certificate of Analysis | Traceability and conformity with the technical approval |
| Composition basis | Active content with explicit units/basis, basicity, density, pH, insolubles, and specified impurities | Like-for-like product comparison and dose-to-volume conversion |
| Source-water quality | Turbidity/TSS, colour, pH, alkalinity, temperature, TOC/organics, metals, algae, and seasonal variation | Dose sweep, pH correction needs, and changing performance risk |
| Treatment process | Rapid mix, flocculation, sedimentation/DAF, filtration, disinfection, and recycle streams | Mixing conditions, floc strength, unit loading, and downstream effects |
| Dosing system | Product concentration, tank/pipe/pump materials, flow, pressure, turndown, calibration, and containment | Feed rate, compatibility, alarms, working stock, and spill response |
| Output criteria | pH, turbidity, aluminium residual, relevant chemical/microbiological parameters, sludge, and regulatory/customer targets | Accept, hold, re-test, or reject against written criteria |
To compare other forms, grades and packages, use the PAC buyer page, industrial liquid PAC and water and wastewater coagulants. Before a dose sweep, also review the PAC-versus-alum comparison against the same process criteria. Select any polymer aid separately through industrial flocculants. Adding polymer without a dose sweep can change the floc, the filtration and the sludge.
How does a PAC jar test become a plant trial?
A jar test screens candidates. However, the permanent setpoint needs plant evidence. Keep the sample identity, dose basis, mixing conditions, settling time, temperature and analytical method. Then the bench result stays traceable when you convert it to dosing-pump output.
- Establish the baseline. Record source, time, temperature, pH, alkalinity, turbidity/TSS, colour, process condition, current coagulant and dose, and finished-water quality.
- Verify the lot. Match label, CoA, density, active basis, and acceptance parameters with procurement documents. Quarantine a lot if its identity is unclear.
- Run a dose sweep. Compare a control, reference product, and candidate on the same sample. Record final pH, floc form and strength, supernatant, settling, filterability, and sludge volume.
- Repeat critical conditions. Test different sources or seasons, organic/algae changes, temperature, and limiting pH or alkalinity.
- Convert the dose basis. Turn the product or active mg/L result into L/h using flow, density, and active content for the correct lot. Do not copy an old pump number.
- Run a controlled plant trial. Begin within the approved envelope, verify pump output, take matched samples, and observe clarifier, filter, and disinfection response.
- Release to routine operation. Approve the setpoint only when finished-water quality, aluminium residual, sludge, consumption, and process stability meet the criteria repeatedly.
Prove the metering equipment with the working liquid. Compare Beta dosing pumps or Watermart dosing pumps after you define flow, pressure, wetted materials, turndown, and standby duty.
What evidence should be retained after lot release?
Minimum records connect the lot, storage tank, setpoint, and water quality. Without that chain, you cannot separate a turbidity or aluminium-residual change from source water, dose, mixing, filter, or product-lot changes.
| Record | Contents | Review trigger |
|---|---|---|
| Receiving and storage | Lot, quantity, seals, package condition, CoA, inspection results, destination tank, and retained sample | New lot, damaged package, contamination, stratification, or exceeded storage period |
| Dosing | Setpoint, calibrated output, treated flow, concentration/density, run hours, and stock consumption | Consumption differs from totalised flow or pump output changes |
| Process quality | Source water, post-coagulation/sedimentation, post-filter, and finished-water points in the procedure | Source, rainfall, algae, pH, turbidity, filter run, or residual changes |
| Sludge | Volume, character, dewatering, filtrate/return, and handling destination | More sludge, poor separation, or a recycle stream disrupts treatment |
| Change control | Reason, tests, approver, trial limits, stop conditions, and final result | Change of grade, lot, supplier, source water, or process configuration |
Liquid PAC for drinking-water FAQs
Does a “drinking” label make PAC safe to use without testing?
No. A product name is not evidence for the lot, dose, or finished water. Verify specifications, CoA, SDS, procurement requirements, jar-test and plant-trial results, relevant residuals, and the filtration and disinfection stages.
Can a liquid PAC dose be copied from another plant?
No. Dose depends on source-water quality, product active content and density, pH and alkalinity, temperature, mixing, separation equipment, recycle streams, and finished-water targets. Test the actual water and record the calculation basis before you change the setpoint.
What is required for an evaluation and quotation?
Send the source and finished-water analyses, the flow and quality variation, the process diagram, the current coagulant and dose, the jar-test results, the reference-product specification/CoA, the dosing-system capacity and materials, the monthly requirement, the storage, the delivery location and the acceptance criteria through the Beta Pramesti Asia contact page.